MM 29: Intermetallic phases II
Donnerstag, 29. März 2007, 11:45–13:00, H16
|
11:45 |
MM 29.1 |
Site occupation and order in γ-TiAl with ternary additions — •Torben Boll, Talaat Alkassab, Zhi-Guo Liu, and Yong Yuan
|
|
|
|
12:00 |
MM 29.2 |
First PAC experiments in MAX phases — •Michael Uhrmacher, Hans Hofsäss, Jens Röder, Pawel Wodniecki, Agnieszka Kulinska, and Michel Barsoum
|
|
|
|
12:15 |
MM 29.3 |
Interface Reaction and its Kinetics of Al and Binary Al-alloys on Mild Steel Substrates — •Werner Fragner, Roman Sonnleitner, Peter Uggowitzer, and Jörg Löffler
|
|
|
|
12:30 |
MM 29.4 |
Non-equilibrium solidification of intermetallic phases in Ni-Al and Ti-Al alloy systems — •Helena Hartmann, Peter Galenko, Hamid Assadi, Sven Reutzel, Roman Lengsdorf, and Dieter Herlach
|
|
|
|
12:45 |
MM 29.5 |
Mechanical milling of single phase beta-Al3Mg2 — •Mira Sakaliyska, Sergio Scudino, Kumar Babu Surreddi, Sebastian Sperling, Carsten Thomas, Michael Feuerbacher, and Jürgen Eckert
|
|
|