MA 21: Magnetic Materials

MA 21.5: Vortrag

Mittwoch, 24. März 2010, 16:15–16:30, H23

Magneto-impedance measurements on iron whiskers — •Matthäus Langosch, Haibin Gao, and Uwe Hartmann — Institute of Experimental Physics, Saarland University, D-66123 Saarbruecken, Germany

After the discovery of the giant magneto-impedance (GMI) effect in 1994, the research on GMI mainly focuses on the enhancement of the effect by developing new materials and on potential applications. But a better understanding of the effect itself is as well needed. GMI measurements on iron single crystals (iron whiskers) with <100> growth direction were carried out at room temperature. The GMI effect of the whiskers has been observed as a function of driving current and frequency. A maximum MI value of 63% was found for the chosen samples having a particularly simple domain structure. MOKE imaging was employed to investigate more clearly the relationship between GMI effect and the respective domain structures. It was found that the magnetic-field-dependent skin effect provides major contributions.

100% | Bildschirmansicht | English Version | Kontakt/Impressum/Datenschutz
DPG-Physik > DPG-Verhandlungen > 2010 > Regensburg